日韩国产欧美制服中文,国产又粗又黄又爽的视频,真实国产乱子伦高清对白,日本欧美亚洲日韩在线视

  • <menu id="fv3ay"></menu>

      <div id="fv3ay"></div>
      <small id="fv3ay"></small>

      
      
      <b id="fv3ay"></b>
      <small id="fv3ay"><th id="fv3ay"><menuitem id="fv3ay"></menuitem></th></small>
      <pre id="fv3ay"><small id="fv3ay"><samp id="fv3ay"></samp></small></pre>

      <dfn id="fv3ay"></dfn>

        Welcome Weihai Global Chemiacl Machinery MFG Co., Ltd.!
        Service Hotline
        0631-5766828
        Advanced Search:
        CONTACT USContact Us


        HOTLINE:0631-5766828

        (7x24)

        Mob:13061173293

        Fax:0631-5766838

        Tel:0631-5766938

        E-mail:

        huanyu01@wh-huanyu.com

        huanyu04@wh-huanyu.com

        huanyu05@wh-huanyu.com


        Address:No.2, South No.1 Road, YangTing Village, HuanCui District


        Hastelloy Reactor
        Your Current Location :HomeProductHastelloy Reactor  ? 5L Hastelloy Reactor
        5L Hastelloy Reactor

        Name:5L Hastelloy Reactor

        Details
        Hastelloy C-276 Alloy

        1. Physical properties
        Density: 8.90g/cm3, specific heat: 425J/kg/k, modulus of elasticity: 205Gpa (21 C)

         
        2. Corrosion resistance
        Harrington C-276 alloy belongs to nickel-based alloy of nickel-molybdenum-chromium-iron-tungsten system. It is one of the most corrosion-resistant modern metal materials. It is mainly resistant to wet chlorine, various oxidizing chlorides, chloride solution, sulfuric acid and oxidizing salts. It has good corrosion resistance in low temperature and medium temperature hydrochloric acid. Therefore, in the past 30 years, in the harsh corrosive environment, such as chemical industry, petrochemical industry, flue gas desulfurization, pulp and paper making, environmental protection and other industrial fields have been widely used.

        Various corrosion data of Harrington C-276 alloy are typical, but they can not be used as specifications, especially in unknown environments. It must be tested before material can be selected. There is not enough chromium in Harrington C-276 alloy to resist corrosion in strong oxidizing environment, such as hot concentrated nitric acid. This kind of alloy is mainly produced in the chemical process environment, especially in the presence of mixed acid, such as the discharge pipe of flue gas desulfurization system. The following table shows the corrosion tests of four alloys in different environments. (All welding specimens are welded by self-fluxing tungsten argon arc welding)